Please use this identifier to cite or link to this item:
https://dspace.iiti.ac.in/handle/123456789/13033
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Kumar, Vikesh | en_US |
dc.contributor.author | Hosmani, Santosh Sattappa | en_US |
dc.date.accessioned | 2024-01-09T06:33:24Z | - |
dc.date.available | 2024-01-09T06:33:24Z | - |
dc.date.issued | 2024 | - |
dc.identifier.citation | Kumar, V., Pruncu, C. I., Wang, Y., Echeverrigaray, F. G., Alvarez, F., Perotti, B. L., Figueroa, C. A., & Hosmani, S. S. (2024). The response of 316 L steel manufactured by selective laser melting route to high-temperature oxidation behaviour: The role of microstructure modification. Materials Characterization. Scopus. https://doi.org/10.1016/j.matchar.2023.113531 | en_US |
dc.identifier.issn | 1044-5803 | - |
dc.identifier.other | EID(2-s2.0-85179587863) | - |
dc.identifier.uri | https://doi.org/10.1016/j.matchar.2023.113531 | - |
dc.identifier.uri | https://dspace.iiti.ac.in/handle/123456789/13033 | - |
dc.description.abstract | The current work examines the effect of 316 L steel's microstructure, which is modified through varying scanning angles with the sample surface (HNS (0°), INS (45°), and VNS (90°)) in the selective laser melting (SLM) method and through surface mechanical attrition treatment (SMAT), on its high-temperature oxidation behaviour (at 600–800 °C) is investigated. We have obtained a deeper understanding of the steel's oxidation behaviour by applying various characterisation techniques. The SMATed steel has a ∼ 1000 μm thick deformed layer containing a gradient microstructure, and its topmost layer contains fine twins and nanograins (∼30 nm). The hardness of this surface is ∼1.65 times the non-treated steel's hardness. All samples follow a parabolic rate law during oxidation. The VNS sample unveils the slowest oxidation rate amid the non-treated samples. SMAT increases the activation energy of oxidation. The distribution of elements across the oxidised samples' cross-section shows discontinuous Cr spreading within the oxide layer on the non-treated samples | en_US |
dc.description.abstract | however, the deformed samples show uniform distribution. Unlike non-SMATed samples, a minute decline in Cr and Mn content is observed underneath the oxide layer on the SMATed samples, confirming their enhanced outward diffusion. The oxide layer on SMATed samples has more Cr- and Mn-rich oxides. These oxides occupy the grain boundaries of the oxidised non-SMATed surfaces, where the micro-pores and cracks are present. Conversely, oxidised SMATed surfaces display uniform, defect-free Cr- and Mn-rich oxides with finer grains. Moreover, the SMATed layer remains reasonably stable during high-temperature oxidation (hardness drop ranges between ∼9 and ∼ 30%). © 2023 Elsevier Inc. | en_US |
dc.language.iso | en | en_US |
dc.publisher | Elsevier Inc. | en_US |
dc.source | Materials Characterization | en_US |
dc.subject | 316 L steel | en_US |
dc.subject | High-temperature oxidation | en_US |
dc.subject | SLM | en_US |
dc.subject | SMAT | en_US |
dc.subject | Thermal stability | en_US |
dc.title | The response of 316 L steel manufactured by selective laser melting route to high-temperature oxidation behaviour: The role of microstructure modification | en_US |
dc.type | Journal Article | en_US |
Appears in Collections: | Department of Metallurgical Engineering and Materials Sciences |
Files in This Item:
There are no files associated with this item.
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.
Altmetric Badge: