Please use this identifier to cite or link to this item:
https://dspace.iiti.ac.in/handle/123456789/9050
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Mohammad, Akbar | en_US |
dc.contributor.author | Ahmad, Khursheed | en_US |
dc.contributor.author | Rajak, Richa | en_US |
dc.contributor.author | Mobin, Shaikh M. | en_US |
dc.date.accessioned | 2022-03-17T01:00:00Z | - |
dc.date.accessioned | 2022-03-21T11:30:49Z | - |
dc.date.available | 2022-03-17T01:00:00Z | - |
dc.date.available | 2022-03-21T11:30:49Z | - |
dc.date.issued | 2018 | - |
dc.identifier.citation | Mohammad, A., Ahmad, K., Rajak, R., & Mobin, S. M. (2018). Binder free modification of glassy carbon electrode by employing reduced graphene Oxide/ZnO composite for voltammetric determination of certain nitroaromatics. Electroanalysis, 30(2), 274-282. doi:10.1002/elan.201700350 | en_US |
dc.identifier.issn | 1040-0397 | - |
dc.identifier.other | EID(2-s2.0-85041837421) | - |
dc.identifier.uri | https://doi.org/10.1002/elan.201700350 | - |
dc.identifier.uri | https://dspace.iiti.ac.in/handle/123456789/9050 | - |
dc.description.abstract | Reduced Graphene oxide/ZnO nanoflowers (rGO/ZnO-NFs) composite has been synthesized in-situ using asymmetric Zn complex (1) as a single-source molecular precursor (SSMP) with GO at 150 °C. The rGO/ZnO-NFs composite was characterized by PXRD, UV-vis, SEM, EDX mapping, TEM and SAED pattern to confirm its purity and morphology. The rGO/ZnO-NFs composite shows uniform distribution of nanoflowers on graphene sheets. The modified glassy carbon electrode (GCE) was fabricated by drop wise layering of the rGO/ZnO-NFs composite at the surface of the GCE without using binder. The binder free modified electrode (GCE-rGO/ZnO) was explored for detection of nitroaromatics such as p-nitro-phenol (p-NP), 2,4-dinitrophenol (2,4-DNP), 2,4-dinitrotoluene (2,4-DNT) and 2,4,6-trinitrophenol (2,4,6-TNP). The fabricated sensor showed remarkable response for the both toxicants and explosives. The LOD, sensitivity and linear range for the studied toxicants and explosives were found to be in a good range: p-NP=0.93 μM, 240 μA mM−1 cm−2 and 0.2–0.9 mM; 2,4-DNP=6.2 μM, 203 μA mM−1 cm−2 and 0.1–0.9 mM; 2,4-DNT=10 μM, 371 μA mM−1 cm−2 and 0.2–0.9 mM; 2,4,6-TNP=16 μM, 514 μA mM−1 cm−2 and 0.2–0.9 mM, respectively. © 2018 Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim | en_US |
dc.language.iso | en | en_US |
dc.publisher | Wiley-VCH Verlag | en_US |
dc.source | Electroanalysis | en_US |
dc.title | Binder Free Modification of Glassy Carbon Electrode by Employing Reduced Graphene Oxide/ZnO Composite for Voltammetric Determination of Certain Nitroaromatics | en_US |
dc.type | Journal Article | en_US |
Appears in Collections: | Department of Chemistry |
Files in This Item:
There are no files associated with this item.
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.
Altmetric Badge: